Aluminum Alloy, 10.0Si - 0.35Mg Stress Relieved, Hot Isostatic Pressed (HIP), Solution Treated and Artificially Aged, Produced by Laser Powder Bed Fusion (L-PBF)
Publication date
2024-08-12
Original language
English
Pages
12
Publication date
2024-08-12
Original language
English
Pages
12
Product information on this site:
Quick delivery via download or delivery service
Buy securely with a credit card or pay upon receipt of invoice
All transactions are encrypted
Short description
This specification covers an AlSi10Mg alloy produced by laser powder bed fusion (L-PBF) additive manufacturing and subjected to stress relief, hot isostatic press (HIP), solution treat, and artificial aging.