Aerospace series - Tartaric-Sulphuric-Acid anodizing of aluminium and aluminium wrought alloys for corrosion protection and paint pre-treatment (TSA)
German title
Luft- und Raumfahrt - Weinsäure-Schwefelsäure-Anodisieren (TSA) von Aluminium und Aluminium-Knetlegierungen für den Korrosionsschutz und zur Vorbehandlung
Publication date
2012-02
Original language
English
Pages
13
Note
The publisher recommends this document in lieu of the withdrawn document
ASD-STAN prEN 4704:2010-11-01
, for which no replacement is available.
Publication date
2012-02
Original language
English
Pages
13
Note
The publisher recommends this document in lieu of the withdrawn document
ASD-STAN prEN 4704:2010-11-01
, for which no replacement is available.
Product information on this site:
Quick delivery via download or delivery service
Buy securely with a credit card or pay upon receipt of invoice
All transactions are encrypted
Cooperation at DIN
Please get in touch with the relevant contact person at DIN if you have problems understanding the content of the standard or need advice on how to apply it.