Standard Test Method for Cathodic Disbonding of Pipeline Coatings Subjected to Elevated Temperatures

German title
Kathodische Ablösung von Rohrleitungsbeschichtungen bei hohen Temperaturen
Publication date
2011 reapproved: 2019
Original language
English
Pages
8

from 73.80 EUR VAT included

from 68.97 EUR VAT excluded

Format and language options

PDF download
  • 73.80 EUR

  • 88.60 EUR

Shipment (3-5 working days)
  • 82.10 EUR

Monitor with the Standards Ticker

This option is only available after login.
Easily subscribe: Save time and money now!

You can also subscribe to this document - together with other important standards in your industry. This makes your work easier and pays for itself after a short time.

Sparschwein_data
Subscription advantages
Sparschwein Vorteil 1_data

Important standards for your industry, regularly updated

Sparschwein Vorteil 2_data

Much cheaper than buying individually

Sparschwein Vorteil 3_data

Useful functions: Filters, version comparison and more

Publication date
2011 reapproved: 2019
Original language
English
Pages
8
DOI
https://dx.doi.org/10.1520/G0042-11R19E01

Quick delivery via download or delivery service

Buy securely with a credit card or pay upon receipt of invoice

All transactions are encrypted

Short description
1.1 This test method describes an accelerated procedure for determining comparative characteristics of insulating coating systems applied to steel pipe exterior for the purpose of preventing or mitigating corrosion that may occur in underground service where the pipe will be exposed to high temperatures and is under cathodic protection. This test method is intended for use with samples of coated pipe taken from commercial production and is applicable to such samples when the coating is characterized by function as an electrical barrier. 1.2 This test method is intended for testing coatings submerged or immersed in the test solution at elevated temperature. When it is impractical to submerge or immerse the test specimen, Test Method G95 may be considered where the test cell is cemented to the surface of the coated pipe specimen. If room temperatures are required, see Test Methods G8 . If a specific test method is required with no options, see Test Method G80 . 1.3 The values stated in SI units to three significant decimals are to be regarded as the standard. The values given in parentheses are for information only. 1.4 Warning Mercury has been designated by EPA and many state agencies as a hazardous material that can cause central nervous system, kidney, and liver damage. Mercury, or its vapor, may be hazardous to health and corrosive to materials. Caution should be taken when handling mercury and mercury-containing products. See the applicable product Material Safety Data Sheet (MSDS) for details and EPA ' s website (http://www.epa.gov/mercury/faq.htm) for additional information. Users should be aware that selling mercury or mercury-containing products, or both, in your state may be prohibited by state law. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.